Home / Coating / Defects

Defects

Holiday testing procedure of internal tank lining.

Holiday testing procedure of internal tank lining.

NACE SP-0188-Holiday testing of internal lining. Equipment-The holiday testing equipment shall be used as high voltage spark tester for coating thickness above 500microns (20mills) ASTM SP D0188.The equipment should be battery operated type and metal brush shall be capable of scanning the tank coating. Calibration of holiday equipment-The holiday detector …

Read More »

Coating defects and others details.

Coating defects and others details.

Coating defects and others details. CHECKING-Checking coating defects of paint failure in which many shall cracks appear in the surface of paint. Checking COALESCING-The settling or drying of an emulsion paint as the water evaporates. COHESION-coating defects of attraction of molecules within a coating ( how it holds together). COLORANT-Concentrated …